The measurement and estimation of the thermo-physical properties of nickel base superalloys.

Author(s):
Quested, P N, Brooks, R F, Chapman, L, Morrell, R, Youssef, Y*, Mills, K C*
Source:
Mater. Sci. Technol., 2009, 25, (2), 154-162
ISSN:
ISBN:
NPL Doc. Ref:
PDB: 5201 | DDB: 1553
Document Type:
Periodical article
DOI:

Note: An asterisk after an author's name indicates a non-NPL author.

Abstract:

Measurement of properties of nickel-base alloys for solidification modelling with a method of estimating properties.